MONEL
INCONEL
logo of AEETHER

AEETHER

INCOLOY
HASTELLOY
UNS R30012

Coballoy Alloy
12

UNS R30012
  1. AEETHER
  2. GRADES
  3. Coballoy 12
you can contact us to buy cobalt alloy 12 by click the button

Get a Free Quote NOW

Learn about Coballoy 12
Products Available
Introduction
Chemical Composition
Data Sheet
Applications
Related Article
Coballoy 12 Raw Materials

Coballoy 12
Raw Materials

  • Bar & Rod
  • Seamless Pipe & Tube
  • Sheet & Plate
  • Disk & Block
you can contact us to buy Coballoy 12 Raw Materials by click the button

Get a Free Quote Now

Coballoy 12 Customized Products

Coballoy 12
Customized Products

  • Processing according to Drawings
  • Processing into any Shape
  • Powder Metallurgy & Casting
  • Turning & Milling & Grinding
you can contact us to buy Coballoy 12 Customized Products by click the button

Get a Free Quote Now

Coballoy 12 Welding Products

Coballoy 12
Welding Products

  • Filler Metal
  • Welding Rod
  • Welding Wire
  • Welding Electrode
you can contact us to buy Coballoy 12 Welding Products by click the button

Get a Free Quote Now

Introduction

logo of solid solution strengthened alloy

Solid Solution
Strengthened Alloy

Cobalt
Chromium
Tungsten
Corrosion
Resistance
87
Mechanical
Behavior
91
Purity
92

Overview

As a leading supplier & manufacturer in China, AEETHER supply cost-effective Coballoy 12 Products.

Coballoy 12 is a cobalt-base alloy having high heat and corrosion resistance with excellent wear and abrasion resistance. Examples include industrial knives for cutting carpets, plastics, paper and synthetic fibers; and saw tips in the timber industry. It is also used for control plates in the beverage industry, pump vanes, bearing bushes and narrow neck glass mold plungers; and for hardfacing of engine valves, pinch rollers in the metal-processing industries and rotor blade edges.

Coballoy 12 could be considered an intermediate alloy between Coballoy 6 and Coballoy 1 resp. Coballoy 3. It contains a higher fraction of hard, brittle carbides than Coballoy 6, and has increased resistance to low angle erosion, abrasion, and severe sliding wear whilst retaining reasonable impact and cavitation resistance.

Coballoy 12 is often used self-mated or running against Coballoy 6 or Coballoy 1 resp. Coballoy 3. The higher tungsten content provides better high temperature properties compared to Coballoy 6, and it can be used at temperatures up to about 700°C.

Corrosion Resistance

The typical electrode potential in sea water at room temperature is approximately -0.3 V (SCE). Like stainless steels, Coballoy 12 corrodes primarily by a pitting mechanism and not by general mass loss in seawater and chloride solutions.

Chemical Composition

Data Sheet

Physical Properties

Density Melting Range
g/cm3 °C
8.5 1200 - 1365

Mechanical Properties

Condition Tensile Strength Yield Strength
(0.2% Offset)
Elongation in 4D Reduction in Area Hardness
MPa MPa % % HRC
Casting 740 580 << 1% / 46 - 51

Applications

Related Article